Vue de la page 20
21
EWM AG /// www.ewm-group.com
pipeSolution
coldArc
coldArc puls
MULTIMATRIX
Perfection is the principle
rootArc
rootArc puls
Powerful arc for rapid, secure welding
with and without gap in all positions.
rootArc: Short arc with perfect weld modelling ca-
pabilities for effortless gap bridging and positional
welding
rootArc puls: The perfect enhancement for
focused heat input for the higher performance
range
coldArc: Heat-reduced, low-spatter short arc for
high dimensional stability welding and brazing,
plus root welding with excellent gap bridging
capabilities.
coldArc puls: The optimum enhancement for the
higher performance range, with focused heat
input – there where the heat is required.
coldArc coldArc puls rootArc rootArc puls pipeSolution
Reduced heat input/
less distortion
    
Reduced energy costs
    
Minimised spatter formation/
less finishing work
    
Gap bridging
    
Reduced harmful emissions/
less welding fumes
    
Arc force
    
Good root formation
    
Root welding in any position
  
Thin panel welding
    
Applications
Unalloyed and low-alloy steels Yes Yes Yes Yes Yes
High-alloy steels Yes Yes Yes Yes Yes
High-tensile fine-grained steels Yes Yes Yes Yes Yes
Brazing (CuSi, CuAl) Yes Yes No Yes No
Brazing (zinc wire ZnAl) Yes No No No No
Dissimilar joint, aluminium with
galvanised steel panel (braze welding)
Yes Yes No Yes No

Good Excellent

Good Excellent